Electroformed Screens for Aerospace Components
Release Date:2026-11-18

Electroformed Screens for Aerospace Components

Overview

A screen that goes into an aircraft component is a small part with a long consequence. It may sit at the inlet of a fuel or hydraulic line, ahead of a pressure sensor, over a vent that has to pass air but hold back contamination, or across an aperture that needs shielding without closing off cooling. Wherever it sits, the screen fixes two things at once: the size of what may pass, and the resistance the line sees. A field that is a few percent off in open area shifts a pressure reading downstream, and a burr on the upstream face releases a particle into a passage that has no room to swallow it.

Electroforming grows the screen as one piece of nickel instead of cutting apertures out of sheet. The aperture field is defined as resist pillars on the plating surface; nickel builds in the open area between them, closes into a continuous sheet at the target thickness, and when the resist is stripped the apertures are open through the metal. An aperture made this way is a void whose wall is a plated surface - smooth, with a taper if the process is set for one, and without the shear lip, recast layer or heat-affected rim that a cut leaves behind. There is no weave, no crossing wire, no braze or adhesive anywhere in the flow path, and every aperture in the field comes off the same pattern.

Etching supports this part as the frame, and only as the frame. A screen thin enough to keep mass low cannot be clamped, aligned and sealed on its own, so it is mounted into a support frame that carries the seal land, the fixing holes, the datum edges and the stiffness the assembly needs to survive handling and vibration. That frame is produced by photo chemical etching, for three reasons: it is thin, the edge that meets a gasket has to be free of burr, and the frame datums and the screen outline must come from the same artwork. The screen itself is electroformed nickel and is never etched. In the delivered set, the etched part is the support frame.

What shapes this work more than any drawing note is repeatability. An aerospace screen is often a replacement item: it may be fitted years after the assembly was first built, and it has to reproduce the flow resistance and the retention the original drawing asked for. That is a process question rather than a print question. Bath composition, pH, temperature, filtration and current density are logged run by run; coupons cut from the panel are measured and filed with the lot record; deposit thickness is checked on the panel while the run is still in the tank. When the bath drifts, the coupon shows it long before the screens reach the bonding station.

Parameter Window

  • Material: electroformed nickel, or nickel-cobalt alloy where a stronger sheet is called for. The screen is a single deposited metal with no coating to lift at an aperture rim. The support frame is nickel or SUS304/316L sheet.
  • Gauge: 0.03 mm to 2.0 mm across the family. Aerospace screens sit at the thin end; the frame is normally the thicker member of the set, agreed at drawing review.
  • Aperture geometry: round, square, slot or hexagonal apertures from the resist pattern; land width, taper and open area follow the plating conditions agreed for the part.
  • Tolerance: quoted against the drawing, with the achievable figure depending on product structure - aperture size, pitch, sheet thickness and open area all move it, so each part is confirmed at review.
  • Surface: matte or semi-bright as agreed, with the upstream and downstream faces specified separately. A screen that sees flow from one side only does not need the same finish on both.
  • Traceability: lot code etched into the support frame, not the screen. A thin screen has no room for a legible mark, and a mark inside the aperture field would alter local flow.

Manufacturing Process / Workflow (8 Steps)

  1. Drawing review. Engineers read the aperture field, open area, frame datum scheme and seal land together, and flag any land too narrow to plate closed or any datum that cannot be reached by the frame.
  2. Pattern generation. The aperture field is written into photoresist as standing pillars on the plating surface, so aperture position, shape and taper are fixed by artwork rather than by a beam path or a punch.
  3. Electrolyte preparation. Nickel sulfamate composition, pH, temperature, filtration and agitation are checked and recorded before the panel enters the tank.
  4. Electroforming. Current density and plating time are set against the thickness target, and deposit thickness is measured on the panel as the run proceeds.
  5. Resist removal and separation. Resist is dissolved out of the apertures, the sheet is taken off the plating surface, rinsed, dried and trimmed to the frame outline.
  6. Frame etching. The support frame is made by photo chemical etching on a separate line: seal land, fixing holes, datum edges and tab windows formed in one pass from the same artwork family as the screen outline.
  7. Assembly and flatness check. Screen and frame are registered on the datum edges, bonded at the land, and the set is checked for flatness, aperture field alignment and seal integrity.
  8. Inspection and packing. Aperture coupons, thickness, open area, appearance and flatness are checked against the drawing, and parts are tray-packed so a thin screen is never stacked under load.

Core Advantages

  1. One pattern, one aperture size. Every aperture in the field comes from the same resist pattern, so the corner of the panel matches the centre and the retention does not drift across the flow path.
  2. A wall that is grown, not cut. No shear lip, no recast layer and no burr on either face, so the screen does not shed metal into a passage downstream of it.
  3. A flat sheet with straight-through apertures. Unlike a woven mesh there is no crimp, no crossing wire and no double thickness at an intersection, so open area and aperture length are set by design rather than by weave.
  4. Mass follows gauge and open area. The screen is a single thin deposit, and every gram is working metal; there is no woven node or wire over/under that adds thickness without adding open area.
  5. The frame takes the load. A screen thin enough to save mass cannot be gripped or compressed against a gasket by itself, so the etched frame supplies the seal land, the fixing points and the stiffness.
  6. One metal, and a lot record to match it. The screen is nickel through its section, with no coating to pit at a rim and no dissimilar joint in the flow path; and each lot carries the coupon data that lets a replacement screen be compared with the one it replaces.

Typical Applications

  • Last-chance screens at fuel, hydraulic and lubricant line inlets
  • Sensor inlet protection screens ahead of pressure and flow elements
  • Breather and vent screens that pass air but hold back contamination
  • Shielding aperture screens for avionics enclosures and connector faces
  • Support screens behind separator and filter media stacks
  • Etched support frames, retaining rings and locating plates for screen sets

Design Notes & Process Considerations

  1. State the aperture as a band plus a test method, not as a single figure. What the line actually experiences is a size distribution, and naming the band and how it will be measured prevents a dispute at incoming inspection.
  2. Balance open area against land width before fixing the pitch. More open area lowers pressure drop but narrows the land, and a land too narrow may not plate closed.
  3. Say which face sees the flow. The upstream face takes the particle load and the downstream face does not, and a drawing that says only "smooth" leaves the inspector to guess.
  4. Treat the seal land as a flatness item. A frame land that is not flat will not compress a gasket evenly, and a leak path around a screen looks exactly like a screen that passes contamination.
  5. Specify cleanliness and handling, not just geometry. Residual resist or a fingerprint on a thin nickel sheet is a rejection at the customer's incoming inspection even when the aperture field measures correctly.
  6. Do not use hardness as an acceptance item. What this process holds is aperture geometry, sheet thickness, open area, surface condition and flatness; a hardness figure on the drawing cannot be held.