Etched Leaf Springs for Precision Devices

Overview

A leaf spring inside a precision device carries two duties that pull against each other. It has to deliver a stated preload across a working stroke, and it has to do that without scraping, sticking or drifting. In an encoder the spring usually appears as a wiper finger or a contact strip that rides a code disc or a signal track under a light, even force. A strip that is bowed changes that force along the track. A slot that is wider at one end changes the spring rate with it. An edge that carries a burr touches first, so the electrical path runs through a line of torn metal instead of across a flat contact face.

Photo chemical etching is used for these parts because the quantities that decide spring behaviour are flat quantities: beam width, beam length, slot width, the radius where a beam meets its frame, and the number of beams carried on one strip. All of them are printed on film and dissolved into the metal rather than cut out of it. There is no punch and no blanking hit, so the edge has no shear band and no roll-over, and nothing presses a bow into thin stock. The edge that remains is the edge the artwork drew, on every piece of the lot.

Flatness is the first gate on thin stock. A strip around 0.05 mm picks up a curve from a single press stroke, and straightening it adds an operation and a fresh set of unknowns. Etching does not squeeze the metal, so strip that arrives flat leaves flat; any bow traces back to the coil's own shape and residual stress rather than to a forming step. Coil identity and incoming flatness are therefore checked at material preparation, where the answer still changes something, instead of being sorted out after the parts are etched.

Batch consistency is the second gate, and it is worth being precise about what the process holds. Spring force is driven hard by thickness, and thickness comes from the rolling mill, not from the etch bath. What etching holds is beam width, slot width and outline: same film, same bath, same line speed, and the first beam of the twentieth lot is defined by the same artwork as the first beam of the first lot. That is why the force-deflection check is read next to the gauge certificate of the coil rather than on its own.

Parameter Window

  • Material: SUS301 in spring temper where the beam has to store and return energy; 304, 304L and 316L where corrosion resistance matters more than rate; 7C27MO2 and 420J2 for hardened strip; titanium TA1, TA2 and TC4 for low mass or chloride exposure; copper C1100 and C1020 where the strip is also the conductor; aluminium 1060 and 5052, and kovar 4J29 or 4J42, where the stack calls for them.
  • Gauge: 0.03 mm to 2.0 mm. Leaf springs usually sit between 0.05 mm and 0.3 mm; heavier stock goes to frames, stiffeners and mounting plates etched in the same blank.
  • Beam and slot: beam width, beam length, slot width, pitch and corner radius are taken from the drawing. Slots are etched through from both faces, so the wall profile follows the resist pattern and the time in the bath.
  • Tolerance: quoted against the drawing, with what is achievable depending on product structure - beam width, slot width, gauge and outline all move it.
  • Edge: contact face and side wall free of burr, dross and roll-over, with no step left across the contact zone.
  • Finish: passivation, pickling or a plating-ready surface as drawn; parts are handled with gloves, packed interleaved, and shipped with the lot record.

Manufacturing Process / Workflow (8 Steps)

  1. Drawing and spring review. Beam length, beam width, slot width, gauge, rate target, stroke and contact force are read together, and a written reply sets out what the drawing asks against what the process holds at that gauge.
  2. Artwork with etch compensation. Beam width and slot width are compensated separately for the gauge, so the finished feature lands on the drawn value rather than on the nominal film value; datum, revision and panel layout are marked on the film.
  3. Material preparation and resist. Grade, temper, coil identity and incoming flatness are checked, the strip is cleaned, and photoresist is laminated on both faces in a controlled environment.
  4. Exposure and development. Beams, slots and outline are printed through the film, the resist is developed, and the metal to be removed is left bare on both faces.
  5. Etching. Panels pass the etchant at a controlled rate; slot width and beam width are held by the resist pattern and the line speed, and any step feature is produced by a controlled half-etch in the same run.
  6. Resist stripping and cleaning. Resist is stripped to completion, the parts are rinsed in stages, given a final rinse in clean water, and dried without leaving marks on the contact face.
  7. Inspection. Beam width, slot width, outline, burr and flatness are checked against the drawing and against a coupon etched on the same panel; the first article also gets a force-deflection measurement.
  8. Packing and handover. Parts are handled with gloves, interleaved, packed flat against crushing, and shipped with the lot record so the next batch can be compared with this one.

Core Advantages

  1. No burr, because nothing is sheared. The edge is dissolved rather than cut, so there is no shear band and no raised roll-over to touch the track first, and no deburring step that could bend a thin beam.
  2. Slot width set by film, not by tool wear. The thousandth piece is cut by the same artwork as the first, so spring rate does not drift as a punch edge would.
  3. Thin stock that stays flat. With no press hit there is no bow pressed into the strip, so 0.05 mm material goes into assembly in the plane it was drawn in.
  4. Compensation matched to gauge. Etch compensation is calculated per thickness and applied to beam and slot separately, so a finished beam measures the drawn width instead of the film width.
  5. Several features in one piece. Multiple beams, an integral frame, locating tabs and root radii can be formed in a single blank, which removes spot welding and riveting from the assembly.
  6. Repeat orders from stored artwork. A spring drawn once is re-etched from the same film and the same parameter set, so beam width and slot width stay comparable between lots.

Typical Applications

  • Wiper fingers and code-disc contacts in optical and magnetic encoders
  • Preload springs for shaft and bearing assemblies inside encoder housings
  • Contact strips and spring fingers in connectors and terminal blocks
  • Detent and return springs in miniature switches and potentiometers
  • Battery contacts and shield fingers in handheld instruments
  • Flat spring washers and leaf elements in sensor and actuator stacks

Design Notes & Process Considerations

  1. Give the rate target together with beam length, beam width and gauge. Force scales with the cube of thickness, so the gauge tolerance of the coil often decides the scatter of a lot more than the etching tolerance does.
  2. State the grade and the temper. Elasticity comes from the strip, and etching only removes metal - it will not turn annealed stock back into spring temper.
  3. Keep slot width in proportion to gauge. A slot close to the stock thickness etches into a waisted wall from two sides, and the beam section is then no longer the rectangle on the drawing.
  4. Put a radius on internal corners. A sharp corner is both a stress riser and a place where fresh etchant exchanges slowly, so it usually comes out blunter or deeper than drawn.
  5. Say how the strip is fed into assembly - a continuous carrier, a reel, or loose parts - and whether tabs or locating holes are needed. Panel layout is arranged around that answer at quotation.
  6. Ask for a force-deflection curve on the first article rather than dimensions alone. A part that measures right and springs wrong is usually a flatness or gauge question, and it is cheaper to find at first article than on a finished instrument.