High-precision metal component manufacturer

Consulting hotline

+086 0755-2708-8292 / 18938693455
Burr-Free Biopsy Screen Etching Service, China
Release Date:2026-11-19

Burr-Free Biopsy Screen Etching Service, China

Overview

A biopsy screen holds a specimen while fluid moves past it, so the screen does two jobs at once. It has to retain what the protocol says to retain, which is a question of pore size and open area, and it has to give the specimen back without dragging fibre, burr or loose debris with it. A pore rim left with a burr catches tissue and holds it through rinsing. A pore that is partly blocked by resist residue changes the open area on that patch of the field, and a plate that still carries etching salts or dried chemistry is a contamination source in a process that is trying to be clean.

Photochemical etching suits that job because of how the metal is removed. There is no punch, no blade and no cutting lubricant anywhere in the process: the plate is coated with resist, the pore array is printed from film, and the metal is dissolved until the pores open through. Nothing is sheared, so nothing is left standing up at the rim. Nothing is machined, so no chip or swarf is pressed into the surface. The pore edge comes out as a smooth, continuous transition rather than a cut edge with a roll-over, and it is the same edge on every pore of the field because every pore is defined by the same film.

Residue control is the part of the service that is easiest to describe and hardest to do consistently. After etching, the resist has to come off completely, including out of fine pores and off the land between them, and the plate has to be rinsed until no etchant remains in the same places. That means a strip and rinse sequence sized to the pore field rather than to the outline of the part, a final rinse in clean water, and an inspection step that looks at the pores under magnification instead of at the plate as a whole.

The China side of the service is about access and repeatability. Buyers abroad are usually working from a drawing and a stack-up that already exists, and what they need is a supplier who will read the drawing before quoting, say plainly which pore sizes and land widths the process holds at a given gauge, run a first article that can be measured, and then hold that result on repeat orders from stored artwork.

Parameter Window

  • Material: SUS304, 304L and 316L as the usual choice for aqueous and wash-down duty; 301 where thin gauge needs more strength; titanium TA1 and TA2 where chloride exposure or weight rules out stainless; copper C1100, aluminium 1060 and 5052, and kovar 4J29 or 4J42 where the housing calls for them.
  • Gauge: 0.03 mm to 2.0 mm. Fine screens sit at the thin end so the pores open through with a short, clean wall; heavier stock suits frames and support plates etched in the same blank.
  • Pore field: round, square or slotted pores, with pore size, pitch, ligament and open area taken from the drawing; the field is checked for size, spacing and open area rather than for appearance alone.
  • Tolerance: quoted against the drawing, with what is achievable depending on product structure - pore size, ligament width, gauge and open proportion all move it.
  • Edge and cleanliness: pore rim free of burr, dross and roll-over; no resist residue and no dried etchant after the final rinse, checked on a sample from the lot.
  • Finish: passivation, pickling or a plating-ready surface as drawn; parts are handled with gloves, packed interleaved, and shipped with the lot record.

Manufacturing Process / Workflow (8 Steps)

  1. Drawing evaluation. Pore size, pitch, ligament, open area, gauge, blank outline and the way the screen is held in its housing are reviewed together, and a written reply sets out what the drawing asks against what the process holds.
  2. Artwork and film. The pore field, edge bands and register features are generated as one artwork set, with the datum, the revision and the panel layout marked on the film.
  3. Material preparation. Sheet is checked for grade, temper and surface condition, cleaned, and laminated with photoresist on both faces in a controlled environment.
  4. Exposure and development. The array is printed through the film, the resist is developed, and the metal to be removed is left bare on both faces.
  5. Etching. The panel passes the etchant at a controlled rate; pore size and edge quality are set by the resist pattern and the line speed, and the run is sampled across the field rather than judged by dwell time.
  6. Resist stripping and cleaning. Resist is stripped to completion, the part is rinsed in stages, given a final rinse in clean water, and dried without leaving water marks in the pores.
  7. Inspection. Pore size, pitch, ligament, open area, burr and residue are checked against the drawing and against a coupon etched on the same panel, with the pore field examined under magnification.
  8. Packing and handover. Screens are handled with gloves, interleaved, packed flat in clean packaging, and shipped with the lot record so the next batch can be compared against this one.

Core Advantages

  1. No burr, because nothing is cut. The pore edge is dissolved rather than sheared, so there is no roll-over and no raised rim for tissue to catch on, and no deburring step that could bend a thin screen.
  2. No lubricant or chip in the process. Etching uses no cutting oil and makes no swarf, so there is no embedded debris to clean out of a fine pore field.
  3. Open area as drawn. Because every pore is printed from the same film, the open area holds across the field instead of drifting where a mechanical tool would have worn.
  4. Residue treated as a process step. Strip, staged rinse and a final clean rinse are run to the pore field, and the result is checked on a sample rather than assumed from the appearance of the plate.
  5. Thin stock that stays flat. Screens down to 0.03 mm come through the line flat, which keeps the field in the plane the housing expects and makes seating predictable.
  6. Repeat orders from stored films. A screen drawn once can be re-etched from the same artwork, so a second lot matches the first without a new setup being proven again.

Typical Applications

  • Specimen retention screens for biopsy cassettes and processing baskets
  • Fine filter screens for laboratory sample preparation
  • Pore plates for cell and tissue handling consumables
  • Support mesh behind a coarser retention screen
  • Screen inserts for diagnostic sample cups
  • Replacement screens matched to an existing housing

Design Notes & Process Considerations

  1. Give pore size with open area and ligament width. A drawing that fixes pore size alone leaves the ligament to the etcher, and the ligament is what decides whether the field etches cleanly.
  2. Keep the ligament wide enough for the bath to work at the gauge chosen. Too narrow a ligament etches through before the field is complete, and the screen fails at the first handling.
  3. Say how the screen is retained in its housing - a rim, a shoulder, a frame etched in the same blank. A retention feature added after etching means a second operation and a second set of tolerances.
  4. State the cleanliness requirement in terms that can be inspected, such as no visible residue at the pore rim under a stated magnification, rather than as a general note.
  5. Tell us if the screen will be passivated, coated or assembled after etching. A coating adds thickness at the pore rim and narrows the opening, so the drawing has to allow for it.
  6. Ask for a coupon on the first article. The coupon is etched and inspected with the lot, so pore size, edge condition and residue are confirmed on the same bath and the same run.
Consult Message
TOP