Overview
A pressure port rarely sees clean media. Scale, sand and fibre travel with the fluid and reach the sensing element unless something small stops them first. A strainer mesh sits at that inlet, often only a few millimetres across, sometimes narrower than the fitting it drops into. At that size two things cannot slip. Every aperture has to pass the same particle, and every edge has to be clean enough not to cut a seal or shed a thread downstream.
Photo chemical etching fits this part because the features that decide filtering are flat ones: aperture diameter, pitch, land width and outline. They are drawn on film and dissolved out of the sheet. No punch touches the metal, so the rim has no shear band and no raised burr facing the O-ring. The aperture keeps the shape the artwork gave it, on the first piece and on the last piece of the run.
Flatness is the first gate on thin stock. A mesh around 0.08 mm takes a curve from a single press stroke, and straightening it adds an operation and a fresh set of unknowns. Etching does not squeeze the sheet, so material that arrives flat leaves flat. Any bow traces back to the coil's own shape and residual stress, not to a forming step. Coil identity and incoming flatness are checked at material preparation, while the answer still changes something.
Batch consistency needs a careful wording. Aperture size comes from the film, the etchant and the line speed; it is not a number measured on every piece. The same film, bath and feed give the thousandth mesh the same aperture form as the first. A blocked port is rarely one cause. Media load, back-flush practice and the particle mix all take a share, and none of them belongs on the etch alone.
Parameter Window
- Material: SUS316L, 304 and 304L where the media is wet or corrosive; SUS301, 420J2 and 7C27MO2 for general industrial service; titanium TA1, TA2 and TC4 for low mass or chloride exposure; copper C1100 and C1020 where the mesh also carries current; kovar 4J29 or 4J42 and aluminium 1060 or 5052 for stacks that call for them.
- Gauge: 0.03 mm to 2.0 mm. Sensor strainers usually sit between 0.05 mm and 0.3 mm; heavier stock goes to mounting rings and support discs etched in the same blank.
- Aperture and pitch: aperture diameter, pitch, land width and array pattern are taken from the drawing. Holes are etched through from both faces, so the wall profile follows the resist pattern and the time in the bath.
- Tolerance: quoted against the drawing, with what is achievable depending on product structure - aperture, pitch and gauge all move it.
- Edge: rim and outer outline free of burr, dross and roll-over, with the ring that meets the seal left smooth so Assembly does not score the gasket.
- Finish: passivation, pickling or a plating-ready surface as drawn; parts are handled with gloves, packed interleaved, and shipped with the lot record.
Manufacturing Process / Workflow (8 Steps)
- Drawing and media review. Media, particle size, flow, aperture, pitch, gauge and mounting method are read together, and a written reply sets out what the drawing asks against what the process holds.
- Artwork with etch compensation. Aperture is compensated separately for the gauge, so the finished hole lands on the drawn value rather than the nominal film value; datum, lot mark and panel layout go on the film.
- Material preparation and resist. Grade, coil identity and incoming flatness are checked, the sheet is cleaned, and photoresist is laminated on both faces in a controlled environment.
- Exposure and development. Aperture array and outline are printed through the film, the resist is developed, and the metal to be removed is left bare on both faces.
- Etching. Panels pass the etchant at a controlled rate; aperture and land width are held by the resist pattern and the line speed, and any step feature comes from a controlled half-etch in the same run.
- Resist stripping and cleaning. Resist is stripped to completion, the parts are rinsed in stages, given a final rinse in clean water, and dried without leaving marks on the rim.
- Inspection. Aperture, pitch, outline, burr and flatness are checked against the drawing and a coupon etched on the same panel; the first article also gets a trial fit into the fitting.
- Packing and handover. Parts are handled with gloves, interleaved, packed flat against crushing, and shipped with the lot record so the next batch can be compared with this one.
Core Advantages
- No burr, because nothing is sheared. The aperture edge is dissolved rather than cut, so the ring facing the seal has no roll-over to score the gasket, and no deburring step can bend a thin mesh.
- Aperture set by film, not by tool wear. The thousandth mesh is opened by the same artwork as the first, so filtering does not drift the way a worn punch would drift it.
- Thin stock that stays flat. With no press hit there is no bow pressed into the sheet, so 0.05 mm material goes into the fitting in the plane it was drawn in.
- Compensation matched to gauge. Etch compensation is calculated per thickness and applied to aperture and land separately, so a finished hole measures the drawn value instead of the film value.
- Several features in one piece. Aperture array, mounting ring, locating tabs and stiffening ribs can be formed in a single blank, which removes welding and riveting from the assembly.
- Repeat orders from stored artwork. A mesh drawn once is re-etched from the same film and parameter set, so aperture and pitch stay comparable between lots.
Typical Applications
- Inlet guard screens in pressure transducers
- Particle barriers over flow sensor probes
- Pre-filter discs ahead of hydraulic and pneumatic ports
- Strainers at the impulse line of differential pressure transmitters
- Fine aperture screens in analytical instrument flow paths
- Isolation mesh discs inside instrument fittings
Design Notes & Process Considerations
- Give aperture together with gauge. When a hole approaches the stock thickness, a two-sided etch waists the wall and the flow section is no longer the circle on the drawing.
- State the media and the particle size. Whether the target is sand or fibre changes the hole form and the array more than a single aperture number does.
- Keep land width in proportion to aperture. A narrow land on thin stock can distort during etch and rinse, and the mesh goes into the fitting already sagged.
- Put a radius on internal corners. A sharp corner is both a stress riser and a place where fresh etchant exchanges slowly, so it usually comes out blunter than drawn.
- Say how the mesh is fitted - pressed in, spot welded, or clamped between two faces - and whether tabs or a mounting ring are needed. Panel layout is arranged around that answer at quotation.
- Ask for a trial fit on the first article rather than dimensions alone. A mesh that measures right but will not seat is usually an outline or edge question, and it is cheaper to find at first article than on the line.