Overview
A filtration screen is judged by two numbers: how evenly the apertures sit across the field, and how much open area survives after the sheet is mounted. Both come out of the same place — the resist pattern and the way etchant reaches the metal. On a photo chemical etching line the coil is cleaned, laminated, exposed through a film tool, developed, then sprayed with etchant from both sides. Metal leaves only where the resist was opened, so each aperture follows the artwork instead of a punch. That matters for mesh. A punched screen carries a burr on the exit face and a taper at every hole, and the die wears from the first stroke. Etching leaves a smooth wall with no roll-over, and one film serves every sheet in the run. A screen mesh etching service in Shenzhen starts with your aperture drawing and ends with a coil or a sheet that matches it.
Parameter Window
- Material: SUS304 / 304L / 316L / 301, copper C1100 / C1020, aluminium 1060 / 5052, titanium TA1 / TA2. Other listed grades reviewed case by case.
- Thickness: 0.03–2.0 mm. Foil under 0.1 mm runs on a carrier frame or with a laminated backing.
- Aperture shape: round, square, slot, hexagon. Walls stay close to vertical when the aperture is not smaller than the sheet thickness.
- Open area: reported as a percentage of nominal area, measured on a fixed field per lot and recorded.
- Web width: coil width and the position of the aperture band are fixed at quotation; both edges keep a strip for clamping.
- Delivery form: coil with winding direction marked, or flat sheet; thin foil interleaved with paper.
Manufacturing Process / Workflow (8 Steps)
- Drawing review. Confirm aperture, pitch, open area, web width and winding direction. Flag the features whose tolerance depends on product structure, and mark where the aperture band meets the edge strip.
- Film tool. Build the artwork with etch-factor compensation, step and repeat it, and place the aperture band and edge margin in one exposure.
- Incoming material. Check grade against the mill certificate, gauge thickness, look for waviness and surface scratches; on coil, note the weld position.
- Cleaning and resist. Degrease, micro-etch, then laminate dry film or dip coat; bake to set.
- Exposure and development. UV passes through the film; developer washes out unexposed resist and opens the aperture sites.
- Etching. Double-sided spray; chemistry, temperature and conveyor speed are set from aperture and pattern density. A coupon is pulled mid-run to measure aperture and web. Wall verticality is fixed here; it cannot be corrected after the strip.
- Resist strip and rinse. Alkaline strip, multi-stage rinse, then blow-dry or oven dry.
- Inspection and packing. Optical measurement of aperture and web, open area calculation, winding check, interleaved packing; sampling follows a fixed field and goes into the lot record.
Core Advantages
- Burr-free on both faces. Metal is dissolved, not sheared, so there is no roll-over at the exit side.
- Aperture set by artwork. The first sheet and the last sheet come off the same film, so pitch does not drift along the run.
- Wall profile is tunable. Spray pressure and chemistry decide whether the wall runs straight or keeps a slight taper.
- No mechanical stress. Thin foil is not stretched or work-hardened, and flat sheet stays flat.
- Aperture change without a die. New hole size or pitch means new film, not new tooling steel.
- One pattern, two delivery forms. The same artwork can leave as coil or as cut sheet.
Typical Applications
- Fuel and lube oil screens: dense aperture band, solid rim left for the seal.
- Hydraulic filter discs: stacked in packs, where aperture and open area set the pressure drop.
- Speaker grilles: aperture array with no visible burr after forming.
- EMI shielding mesh: small pitch and narrow web, where web breakage is the main risk.
- Intake and dust screens: large open area, where web width and winding direction decide fit.
- Fine sieving mesh: regular aperture for powder grading and lab screening.
Design Notes & Process Considerations
- Aperture against thickness sets the wall. When the aperture approaches the sheet thickness, undercut takes a larger share and the wall turns curved. Allow for that in the drawing and confirm the allowance with a test coupon.
- Higher open area means narrower web. Etchant attacks the web from both sides, so add width where the web carries load. A web narrow enough can break before resist strip, and redrawing is cheaper than reworking.
- Dense fields exchange etchant slowly. Add a flow path outside the aperture band or etch in groups, rather than pushing spray pressure up.
- Keep the aperture band at least two web widths from the coil edge; otherwise the edge distorts during winding and unwinding.
- Foil below 0.05 mm is better run as sheet on a frame. Coil tension pulls apertures out of round.
- Write the burr requirement as a measured limit, not as "no burr". A number you can inspect is a number we can hold. State the wall finish as well.