Overview
A lead frame usually fails at the finger tip, not at the frame body. Stamping leaves a rolled edge there, plating builds up on that edge, and the gap between two fingers closes. Etching takes the metal away in a bath instead of shearing it, so the tip ends square and the finger face stays flat. That is the whole reason this process is used for fine pitch work. We run lead frame etching in Shenzhen on strip and on sheet, for programs where the pitch and finger width sit below what a stamping die can hold without wearing out. What you send decides what we can promise: artwork, alloy, thickness, temper and carrier format. Nothing else on the drawing changes the outcome as much as those five.
Parameter Window
- Alloy — copper C1100 and C1020 for current-carrying frames; expansion alloys 4J42 and 4J29 for glass-to-metal seals; stainless 7C27MO2, SUS304 and SUS301 where stiffness or corrosion resistance drives the choice.
- Thickness — 0.03 mm to 2.0 mm. Lead frame work sits on the thin side of that band, and we do not quote below 0.03 mm.
- Pitch and finger width — taken from your drawing, not from a catalogue. Whether a layout can be etched depends on the ratio of finger width to strip thickness, and on how much of the gap is left open.
- Temper — soft, half hard and hard strip all run. There is no anneal after etching, so the temper you supply is the temper the part keeps.
- Carrier format — reel with carrier tape and index holes, or flat sheet. For reel work we need web width, winding direction and the rule for splices.
- Inspection — finger width, pitch, coplanarity, burr and pre-plate surface condition, measured against the zones marked on your drawing.
Manufacturing Process / Workflow (8 Steps)
- Drawing review. We check pitch, finger width, tie bar position, index holes and carrier dimensions, then mark which edges need etch compensation.
- Artwork and film. Compensation follows the etch factor of the alloy. Fine finger zones get their own correction, because they lose more width per side than the body does.
- Dry film lamination. Strip is laminated continuously; roller temperature and pressure are held so no air is trapped under the film at the finger tips.
- Exposure. Both sides are exposed against the index holes as the datum. On fine pitch panels the operator checks offset at the finger zone, not at the panel edge.
- Development. Unexposed resist washes out and the metal that will become the gap is left bare.
- Etching. Spray pressure, conveyor speed and bath chemistry are set from strip thickness and finger width. Sideways cut, which sets the final finger width, is fixed at this step.
- Resist strip and rinse. Film comes off, then multi-stage water rinse. Residue left here shows up later as a skip in the plating line.
- Inspection and packing. Finger width and pitch are measured, coplanarity checked on a flat plate, burr checked at the tip. Reel work is wound to the agreed carrier format; sheet work is interleaved and boxed.
Core Advantages
- No stamping marks. There is no die edge and no shear band, so the finger face stays flat and needs no polishing before plating.
- Stable fine pitch. Finger width is set by the film. Re-run the same artwork and the width repeats, with no die wear to chase.
- Burr-free tips. The cut closes chemically instead of tearing, so plating cannot pile up on a rolled edge and bridge the gap.
- Coplanarity by control, not by straightening. No mechanical shear means no locked-in stress; flatness comes from web tension and handling, not from a leveling pass.
- Cheap to revise. Move a pitch or add a finger by editing artwork. No tooling to cut, no die to modify.
- One line, several alloys. Copper, expansion alloy and stainless run through the same process, which matters when a frame stack mixes materials.
Typical Applications
- QFN and DFN packages, where the gap between fingers carries the standoff
- Small outline frames for sensors and MEMS packages
- LED lead frames and die pads on thin copper
- 4J42 and 4J29 frames for glass-to-metal sealed packages
- Connector terminals, spring contacts and fine pitch pin rows
- Bare frames supplied to a nickel-palladium-gold plating line
Design Notes & Process Considerations
- Read finger width and thickness together. As finger width approaches strip thickness, sideways cut takes a larger share and the finished finger comes out narrower than drawn. That loss has to be built back into the film.
- Tie bars carry the stiffness. Leave enough tie bar either side of a fine finger field, or the strip sags as it runs through the line and the reel winds unevenly.
- Etching works from both faces. The finger wall comes out slightly waisted through the thickness. If you need a near-vertical wall, say so before artwork is released.
- Round the sharp corners. A sharp internal corner etches away first and drifts from the drawing. A defined radius holds its size.
- Match the plating pre-treatment to an etched surface. The surface after etching is chemical, not rolled. Acid dip and activation times set for rolled strip are usually too long here and cause skip plating at the finger tip.
- Carrier and index holes follow the assembly equipment, not the etch tolerance. Set them from the pick-and-place or die bonder that will use the reel.