High-precision metal component manufacturer

Consulting hotline

+086 0755-2708-8292 / 18938693455
Electroformed Screen Mesh for Solar Cells
Release Date:2026-11-23

Electroformed Screen Mesh for Solar Cells

Overview

Screen printing lays the contact grid on a solar cell. The squeegee pushes paste through a screen, and the openings decide where the paste lands and how much of it passes. A front grid carries fine fingers and a few busbars; the rear side takes a heavier deposit. Line width and deposited height follow the opening, not the squeegee. When openings vary across the screen, the fingers vary with them: thin lines here, fat lines there, and a spread between cells that shows up at test.

The working screen is electroformed nickel. A flat substrate carries the grid as openings in resist, and nickel grows into those openings until the foil reaches gauge. Each aperture is bounded by a resist wall, so its wall is grown rather than punched: straight, smooth, with no roll-over from a two-sided etch. Paste slides along that wall and releases on the cell. Gauge comes from plating time and current density, so one bath can grow a fine grid and a coarse grid at the gauge the printer needs. Tension is where this pays off. A foil of even gauge takes an even pull when it is stretched; a foil that thins in patches relaxes in those patches and the print drifts between strokes.

Photo chemical etching is in this part number too, but on the registration frame only. The frame outline, locating holes, notches that set print position, the window that exposes the active area and the glue land are etched from stainless steel or aluminium. It is a flat part defined by an outline and a step, which is what etching handles well. It is not the process that forms the mesh openings. Merge the two on one drawing and a single tolerance band lands on a grown foil and an etched frame; neither process will hold it.

At quotation, separate what the process holds from what the printer sets. Openings follow the patterned substrate, gauge follows plating, and flatness follows the substrate plus low deposit stress. Tension is a property of the stretched assembly - foil gauge, frame land and bond method together - not a number the bath delivers alone. Nickel hardness comes from bath chemistry and is not dialled to a drawing note. A repeat lot grows from the retained substrate and the same bath recipe as the first one.

Parameter Window

  • Screen material: electroformed nickel as standard; nickel-cobalt alloy where the grid must resist wear over long print runs. The grown screen is nickel-based only, with no copper, gold or silver in it.
  • Registration frame material: SUS304, 304L and 316L for general use; 420J2 and 7C27MO2 where the frame needs more stiffness; aluminium 1060 and 5052 for low mass; titanium TA1 and TA2 for chloride exposure; kovar 4J29 and 4J42 where the frame bonds into a ceramic fixture.
  • Gauge: screen foil from 0.03 mm upward; registration frame from 0.03 mm to 2.0 mm, the frame usually heavier than the foil it carries.
  • Grid pattern: finger width, busbar width, pitch and open area are taken from the drawing. The wall grows into the resist opening, so it follows the pattern rather than an etch dwell.
  • Tolerance: quoted against the drawing, with what is achievable depending on product structure - finger width, pitch, foil gauge and frame geometry all move it.
  • Edge and finish: aperture walls free of burr and dross; frame edges clean, locating holes and half-etched steps as drawn; cleaning and passivation as specified, glove handling, flat packing.

Manufacturing Process / Workflow (8 Steps)

  1. Print review. Paste type, cell size, grid design, target line width and deposit height, strokes per minute and frame interface are read together, and a written reply sets the drawing against what the process holds.
  2. Drawing split. Grid and frame go on separate sheets. Finger width, open area and foil gauge sit on one; outline, locating holes, window and glue land on the other.
  3. Substrate patterning. Photoresist is applied to a flat substrate and exposed so the grid exists as openings in the resist; substrate flatness is checked before plating, because the foil inherits it.
  4. Nickel electroforming. Bath, temperature, current density and time are set for the required gauge; nickel grows in the resist openings, and deposit stress is kept low so the released foil lies flat.
  5. Release and clean. The foil is peeled from the substrate, rinsed in stages and dried flat, then checked for curl before it is stretched.
  6. Registration frame etching. The frame is produced by photo chemical etching: outline, locating holes, registration notches, the exposed window and the half-etched glue step all come from one artwork.
  7. Stretch, bond and inspect. Foil is pulled onto the frame and bonded on the land; line width, pitch, open area, gauge, flatness and aperture walls are measured, and a print trial checks paste release.
  8. Pack and handover. Screens are handled with gloves, packed flat with spacers, and shipped with the lot record and a retained coupon so a repeat order can be compared with this one.

Core Advantages

  1. Even openings across the foil. The grid comes from one patterned substrate, so a finger at the edge matches one in the middle and printed line width stays even over the whole cell.
  2. Paste passes cleanly. A grown wall is straight and smooth, so paste releases instead of hanging at a rough edge, and the apertures resist clogging over a print run.
  3. Tension stays even. The foil grows to a uniform gauge, so a stretched screen pulls evenly and the grid does not shift between strokes.
  4. No burr at the aperture. There is no shear band or roll-over to catch paste or mark the cell surface.
  5. Frame and grid on one datum. The registration frame is etched from the same drawing set, so holes, window and active area line up when the foil is bonded.
  6. Repeat runs trace back. Substrate and bath recipe are retained, so grid and gauge of a repeat lot match the first one - the practical value of this screen in volume.

Typical Applications

  • Front-side contact printing on mono and multi-crystalline cells
  • Rear-side metallization screens for thick contact paste
  • Busbar and finger grid printing on large-format wafers
  • Half-cell and shingled cell metallization screens
  • Print trials and line-width studies on new grid designs
  • Registration frames for screen printers in pilot lines

Design Notes & Process Considerations

  1. Give the grid and the paste together. Finger width and open area set deposited volume; paste rheology decides whether that volume releases. One without the other is not enough to quote.
  2. Keep open area in proportion to foil gauge. A narrow finger in a thick foil closes before the deposit reaches gauge, so a dense, deep grid is a plating question rather than a drawing question.
  3. Say how the foil is bonded to the frame. A glued joint needs land width; a welded tab needs a flange; a clamped seat needs a step. The etched frame follows that answer.
  4. Ask for released flatness together with a measuring method. Flatness comes from the substrate and deposit stress, and a number without a method cannot be checked at either end.
  5. Treat nickel hardness as a bath property. It follows the bath chemistry and is not set to a figure on request, so ask what the bath delivers before writing a hardness note.
  6. Keep the screen and the frame on separate drawings. One is grown, one is photo chemical etched; combining them invites tolerances that suit neither process.
Consult Message