High-precision metal component manufacturer

Consulting hotline

+086 0755-2708-8292 / 18938693455
Electroformed Micro-Perforated Screens for Audio
Release Date:2026-11-19

Electroformed Micro-Perforated Screens for Audio

Overview

Every audio product has a hole field somewhere in its acoustic path: the front of a driver, the outlet of an earpiece, the inlet of a microphone, the vent of a sealed enclosure. That screen does two jobs at once. It keeps dust, lint and stray metal out of a diaphragm that has almost no clearance, and it sits in the sound path, where it adds a small acoustic resistance and a small mass. Both of those are design values, not side effects: the tuning was done with a screen in place, and a unit whose screen differs in open area or in hole length will not match the curve the acoustic engineer signed off.

Electroforming produces that hole field by growth rather than by punching or cutting. Holes are defined as resist pillars on the plating surface; nickel builds in the open area between them, closes into a continuous foil at the target gauge, and once the resist is stripped the holes run clean through the metal. Each hole wall is a plated surface, so it is smooth and free of the shear lip, recast rim and clinging burr that a mechanical cut leaves. Because the field is a single deposit from a single artwork, the hole at one corner of the panel and the hole at the other are the same hole, and that is what keeps unit-to-unit sensitivity inside a narrow band.

Etching is used here for the mounting frame, and for nothing in the acoustic path. A foil thin enough to stay acoustically transparent cannot carry a glue line, a snap feature and two screw bosses on its own, so it is bonded into a frame that provides the bond land, the location to the housing and the stiffness to survive handling and drop. That frame is made by photo chemical etching: it is thin, the edge that meets the bond line has to be burr-free, and its datums must come from the same artwork family as the screen outline. The screen itself is electroformed nickel; the etched part is the frame.

Volume is where this part is won or lost. A single speaker screen is unremarkable; getting a hundred thousand of them to sound the same is a process achievement. The hole field is stepped and repeated across a panel so one plating run yields many screens, deposit thickness is measured on the panel while it is still in the tank, and coupons cut from the panel are measured and filed with the lot. The frame is etched on a separate line in parallel, so the two streams meet at the bonding station instead of one waiting on the other.

Parameter Window

  • Material: electroformed nickel, or nickel-cobalt alloy where a stronger foil is needed at the same gauge. The screen is a single deposited metal with no coating to flake at a hole edge. The mounting frame is nickel or SUS304/316L sheet.
  • Gauge: 0.03 mm to 2.0 mm across the family. Audio screens sit at the thin end, because added mass costs sensitivity; the frame is normally the thicker member of the set.
  • Hole geometry: round, square or slotted holes on a staggered or square pitch, all set by the resist artwork. Hole size, land width and open area are agreed together at drawing review.
  • Tolerance: quoted against the drawing, with the achievable figure depending on product structure - hole size, pitch, foil thickness and open area all move it.
  • Acoustic target: open area and hole length are stated as a target with the measurement method agreed in advance, so the finished screen can be checked the same way the design was modelled.
  • Traceability: lot code etched into the mounting frame. A foil thin enough for audio has no room for a legible mark, and a mark in the hole field would change local resistance.

Manufacturing Process / Workflow (8 Steps)

  1. Drawing review. Engineers read the hole field, the open-area target, the frame bond land and the housing location together, and flag any land too narrow to plate closed or any hole group too close to the bond line.
  2. Pattern generation. The hole field is stepped and repeated across the panel in photoresist as standing pillars, so hole position, size and pitch are fixed by artwork rather than by a punch or a laser path.
  3. Electrolyte preparation. Nickel sulfamate composition, pH, temperature, filtration and agitation are checked and recorded before the panel enters the tank.
  4. Electroforming. Current density and plating time are set against the gauge target, and deposit thickness is measured on the panel as the run proceeds so the run can be corrected before it ends.
  5. Resist removal and separation. Resist is dissolved out of the holes, the foil is lifted off the plating surface, rinsed, dried and trimmed to the frame outline.
  6. Frame etching. The mounting frame is produced by photo chemical etching on a separate line in parallel with plating: bond land, location features and fixing points formed in one pass from the same artwork family.
  7. Bonding and flatness check. Foil and frame are registered, bonded at the land, and the set is checked for flatness, hole field alignment and bond integrity.
  8. Inspection and packing. Coupon holes, thickness, open area, appearance and flatness are checked against the drawing, and parts are tray-packed so a thin foil is never stacked under load.

Core Advantages

  1. One artwork, one hole. Every hole in the field is formed under the same conditions, so the acoustic resistance of the first unit matches the last one in the run.
  2. A wall that is grown, not cut. No burr on either face, so the screen does not shed metal onto a diaphragm and does not scratch a housing during assembly.
  3. Thin gauge at a given open area. The screen is a single deposit, so open area is bought with hole geometry rather than with extra thickness, and added mass stays low.
  4. Open area set by design, not by weave. There is no crimp and no crossing wire, so the resistance the acoustic model assumed is the resistance the part delivers.
  5. The frame takes the bond and the load. A foil thin enough to be acoustically transparent cannot carry a glue line and two screw bosses, so the etched frame supplies the land, the location and the stiffness.
  6. One metal, one lot record. The screen is nickel through its section, with no coating to flake at a hole edge; each lot carries coupon data, so one production batch can be compared with the next.

Typical Applications

  • Driver front screens for in-ear, on-ear and portable speakers
  • Earpiece and receiver outlets in handsets and headsets
  • Microphone inlet covers and wind screens
  • Vent screens for acoustic ports and tuned enclosures
  • Dust screens behind decorative grilles
  • Etched mounting frames, retaining rings and locating plates for screen sets

Design Notes & Process Considerations

  1. Specify the acoustic target, not just the hole size. Open area and hole length set the resistance, and a drawing that names only a hole size leaves the acoustic result to chance.
  2. Balance open area against land width before fixing the pitch. More open area lowers resistance but narrows the land, and a land too narrow may not plate closed.
  3. Keep the bond land outside the hole field. Adhesive that creeps into a hole closes it, and a closed patch reads as a local rise in resistance that no inspection of the hole field will explain.
  4. Say which face looks at the diaphragm. The face that can touch a moving diaphragm is the one that must be free of anything that could rub; both faces are plated clean, but the note belongs on the drawing.
  5. Write cleanliness and handling into the requirement. Residual resist or a fingerprint changes local resistance even when the hole field measures correctly at incoming inspection.
  6. Do not use hardness as an acceptance item. The process holds hole geometry, foil thickness, open area, surface condition and flatness; the deposit is not heat treated to a hardness target, so a hardness figure cannot be held.
Consult Message