Overview
A charging connector is a current path with a mechanical job. Inside the gun, the inlet and the battery-side interface there is a stack of copper parts - contact terminals, spring fingers, busbar ends, ground tabs - and each one has to sit in a housing, mate with a counter-contact, carry current without a hot spot, and take a plated finish before it goes into the assembly. The outline of that part decides how much surface faces the mating contact, how far a finger deflects, and whether the part seats flat on its insulator.
That is the work this etching service in Shenzhen is built around: forming those outlines chemically, from a drawing, on copper sheet, in sample quantities and in production batches from the same line. The panel is coated with photoresist, the terminal profile is printed from artwork, the exposed metal is dissolved, and what remains is the terminal at the drawn outline with its slots, relief cuts and locating windows already in it. There is no cut edge to deburr, no shear zone work-hardened at the rim, and no flatness lost to a mechanical stroke.
For a plated terminal the condition of the substrate matters as much as the outline. Etching does not fold or smear the surface, so the nickel or tin layer that follows sits on clean, uniform metal. Edges come out square and free of the hanging burr that survives a plating barrel and later shows up as a nodule, or as a sharp point that damages a mating contact. Where the part is masked for selective plating, the mask outline is taken from the same artwork family, so the plated band lands where the drawing puts it.
The service is regional as well as technical. Terminals are often designed in one place, prototyped in another and built in a third, and a Shenzhen base shortens the loop between a drawing revision and a part in hand. A drawing pack is reviewed for material, gauge, feature size, land width and plating scheme; the points that cannot be held are raised before anything is etched; the part then runs as a sample lot, is measured, and only after that is released to batch. Copper grade, temper and plating spec travel with the lot record.
Parameter Window
- Material: copper C1100 and C1020 for current-carrying terminals and busbar ends; SUS304/316L where a spring clip or a shield plate is etched in the same set; aluminium 1060/5052 for housing-side plates; kovar where a glass seal is involved.
- Gauge: 0.03 mm to 2.0 mm. Terminal work sits between thin foil contacts and heavier busbar stock, and the two ends of that range behave differently in the etch bath.
- Outline features: terminal profile, contact fingers, slots, relief cuts, locating windows and plating mask openings, all taken from one artwork set.
- Tolerance: quoted against the drawing, with the achievable figure depending on product structure - copper gauge, feature width, land width and open proportion all move it.
- Edge condition: square edge, no hanging burr, no rolled-over rim; the criterion for a plated part is written on the drawing and checked against a coupon from the same panel.
- Traceability: lot code on the frame or the carrier strip, with coupon data for outline, gauge and edge condition filed per lot.
Manufacturing Process / Workflow (8 Steps)
- Drawing evaluation. Material, gauge, feature size, land width, plating scheme and datum scheme are read together, and a written reply comes back on what the drawing asks for against what the process can hold.
- Artwork and film. The terminal outline and every internal cut are generated as one artwork set; where the part is selectively plated, the mask outline is taken from the same file.
- Material preparation. Copper is checked for grade, temper and surface condition, cleaned, and laminated with photoresist on both faces.
- Exposure and development. The profile is printed through the film and the resist is developed, so the metal to be removed is bare.
- Etching. The panel passes through the etchant at a controlled rate; cut width and edge squareness are held by the resist pattern and the line speed, and the run is monitored rather than left to time alone.
- Resist stripping and cleaning. Resist is removed, the part is rinsed and dried, and any mask opening is verified before plating.
- Inspection. Outline, feature size, flatness, burr and surface condition are checked against the drawing and against the coupon cut from the same panel.
- Packing and handover. Parts are interleaved and packed flat so a thin terminal does not take a set in transit, and the lot record ships with the box.
Core Advantages
- One outline across the lot. The profile comes from a single artwork set, so terminal width, finger length and slot position do not drift from piece to piece.
- A plating-ready edge. No hanging burr and no smeared rim means the deposit builds evenly over the edge, with no sharp point left to damage a mating contact or a seal.
- No mechanical stress in the part. Flatness arrives with the sheet and is not disturbed by a shear or a press stroke, which matters for a contact that has to seat on an insulator.
- Revisions move at artwork speed. A longer finger or an added relief cut is a new film rather than a new production setup, so a prototype loop stays short.
- Small features in the same pass. Slots, windows and mask openings are etched with the profile, so there is no second operation and no re-registration error between them.
- Local loop, documented lots. Evaluation, sample and batch run from the same Shenzhen base, and each lot carries the coupon data an incoming inspection needs.
Typical Applications
- Contact terminals and spring fingers in charging guns and inlets
- Busbar ends and laminated connection plates for battery packs
- Ground tabs and shield plates in charging modules
- Contact carrier strips for connector assembly
- Terminal plates with integral slots and relief cuts
- Etched plating masks and locating frames for terminal sets
Design Notes & Process Considerations
- Send the plating spec with the drawing. The finish sets the edge criterion, and an edge accepted under a tin flash is not necessarily accepted under a hard nickel.
- Give the burr limit as a number plus a measurement method, not as "burr-free". Both faces see the etchant, and the inspector needs a figure to compare against.
- Note the rolling direction of the copper if flatness is critical. Grain direction and temper set the starting flatness, and etching does not add stiffness.
- Keep the land between two openings wide enough for the bath to work. A land that is too narrow etches through before the outline is finished.
- Put the datum on an etched feature rather than on a sheared edge, or the reference shifts with the material lot.
- Carry the revision and the plating note in the same file. A terminal re-etched to an old revision will still fit the housing and then fail at the plating stage.