Overview
A centrifuge screen separates by geometry, not by a membrane. What passes is decided by the pore, and the pore has three properties that have to hold together across the whole field: roundness, pitch and open area. An oval pore passes a particle the drawing would have retained, so roundness is a cut-size question rather than a cosmetic one. Pitch decides how much open area the field carries and how wide the ligament between pores is, and a pitch that wanders leaves a soft band where the screen flexes and eventually tears. Open area sets throughput and pressure drop, and in a basket it also sets how dry the cake comes off.
Etching forms those three properties from one artwork, which is why the process suits a screen that has to behave the same at the top of the basket as at the bottom. The panel is resist-coated, the pore array is printed from film, and the metal is dissolved until the pores open through. Because the pattern is projected rather than punched, pore shape and pitch are set by the drawing across the full developed width, and there is no punch wear to shift the last row relative to the first. The wall of each pore comes out square, with no shear zone and no burr left to trap fibre or hold product after a wash.
Rigidity is the constraint that shapes the drawing. Etching removes metal, so it cannot add stiffness; what it can do is keep the stiffness the design asked for, evenly. A screen holds its form through gauge, through the ligament between pores and through features etched into the same blank - a solid edge band, an intermediate rib, a heavier land at the clamp ring. Those are cut in the same pass as the array, so the field and its reinforcement are one piece, with no weld line to corrode or to fatigue under a backwash pulse.
The regional part of the service matters because a screen is usually a rebuild item as well as a new-build item. A plant measures a worn screen, sends a sketch or a sample, and needs a replacement that matches the basket it sits in. A Shenzhen base reviews the developed blank, checks the weld or clamp allowance at each end, and returns a written reading of what the drawing can hold before anything is etched. Samples and batches run on the same line, so a trial screen and the production screen come from one artwork set.
Parameter Window
- Material: SUS304 and 316L for food, pharmaceutical and wash-down duty, 301 where higher strength is needed in thin gauge, titanium TA1/TA2 for chloride or oxidising service, aluminium 5052 for light non-wetted baskets, copper C1100 for specific non-ferrous duty.
- Gauge: 0.03 mm to 2.0 mm. Centrifuge screens normally sit in the heavier part of that range; the thin end applies to fine support meshes and to filter layers behind a coarser screen.
- Pore and pitch: round, square or slotted pores, with diameter, pitch and ligament set by the drawing; the array is checked for roundness and for pitch drift across the developed width.
- Tolerance: quoted against the drawing, with the achievable figure depending on product structure - gauge, pore size, ligament width and open proportion all move it.
- Edge condition: square pore wall, no burr, no rolled-over rim; the edge criterion is written on the drawing and checked against a coupon from the same panel.
- Blank and finish: developed blank with weld or clamp allowance, solid edge bands and ribs etched in place; passivation or pickling available on stainless, with the finish stated per drawing.
Manufacturing Process / Workflow (8 Steps)
- Drawing evaluation. Material, gauge, pore size, pitch, ligament, open area, developed length and end allowance are read together, and a written reply sets out what the drawing asks against what the process holds.
- Artwork and film. Pore array, edge bands, ribs and clamp lands are generated as one artwork set, with the array datum and the revision marked on the film.
- Material preparation. Sheet is checked for grade, temper and flatness, cleaned, and laminated with photoresist on both faces.
- Exposure and development. The array is printed through the film and the resist is developed, leaving the metal to be removed bare on both sides.
- Etching. The panel passes the etchant at a controlled rate; pore size, roundness and ligament width are held by the resist pattern and the line speed, with the run sampled across the width rather than left to time.
- Resist stripping and cleaning. Resist is removed, the part is rinsed and dried flat, and any passivation step follows before packing.
- Inspection. Pore size, roundness, pitch, ligament width, open area, burr and flatness are checked against the drawing and against a coupon etched on the same panel.
- Packing and handover. Blanks are interleaved, packed flat and shipped with the lot record, so a thin screen does not take a set before it is rolled or clamped.
Core Advantages
- Pore geometry from one artwork. Roundness and pitch come from the film rather than from tool wear, so the first row and the last row of a wide blank measure the same.
- Open area as drawn. Because the array is projected, open area holds across the developed width instead of drifting where a mechanical tool would have worn.
- No stress in the blank. Etching leaves no shear zone and no rolled rim, so a screen stays flat until it is formed and does not spring back against a clamp ring.
- Ribs and bands in the same pass. Edge bands, intermediate ribs and clamp lands are cut with the array, giving rigidity where the design wants it without a welded-on stiffener.
- A bore that cleans. Square pore walls without burr release cake and rinse clear, which matters on a machine that is cleaned in place between product runs.
- Replacement without a new setup. A worn screen is re-etched from the same artwork, so a rebuild matches the basket instead of being trimmed to fit.
Typical Applications
- Basket screens for batch filtering centrifuges
- Screen sections for decanter centrifuge bowls
- Conical screens for screening centrifuges
- Fine support meshes behind a coarse drain screen
- Slotted screens for dewatering and classification
- Replacement screen blanks cut to a measured worn part
Design Notes & Process Considerations
- Give the pore size with the open area, not instead of it. Two screens can share a pore size and differ in throughput because the pitch differs.
- Keep the ligament wide enough for the bath to work. A ligament that is too narrow etches through before the array is complete, and the screen fails at the first backwash.
- Put the weld or clamp allowance on the drawing as a solid band. The band is etched in the same pass, and a band added later means a second operation.
- State the developed length and how it was measured. A blank etched to a nominal length and formed to a measured basket is where fit problems begin.
- Ask for a tapered pore wall only if the duty needs it. A double-sided etch can leave a slight taper that helps flow and rinse, but it also changes the effective open area.
- Note the array orientation and the revision on the drawing. A rotated array changes both the edge closure and the ligament at the clamp band.